The material landscape in one view.
A fast relative guide for the first screening conversation. “Excellent” does not mean universal compatibility.
| Polymer | Heat | Chemical Breadth | Oil / Fuel | Water / Steam | Ozone / Weather | Abrasion / Mechanics |
|---|---|---|---|---|---|---|
| FFKM Perfluoroelastomer | Excellent | Excellent | Excellent | Good* | Excellent | Fair |
| FKM Fluoroelastomer / Fluorocarbon | Excellent | Excellent | Excellent | Fair | Excellent | Good |
| FEPM TFE-Propylene / Aflas®-type | Excellent | Excellent | Good | Excellent | Excellent | Fair |
| FVMQ Fluorosilicone | Good | Good | Excellent | Poor | Excellent | Fair |
| HNBR Hydrogenated Nitrile | Very Good | Good | Very Good | Fair | Good | Excellent |
| VMQ Silicone Rubber | Excellent | Fair | Poor | Fair* | Excellent | Poor |
| EPDM Ethylene Propylene Diene Rubber | Very Good | Good | Poor | Excellent | Excellent | Good |
| NBR Nitrile / Buna-N | Good | Fair | Excellent | Fair | Poor | Very Good |
| CR Chloroprene / Neoprene-type | Good | Fair | Fair | Good | Excellent | Good |
| AEM Ethylene Acrylic Elastomer | Very Good | Fair | Very Good | Fair | Excellent | Good |
| ACM Polyacrylate Rubber | Very Good | Fair | Excellent | Poor | Excellent | Fair |
| ECO Epichlorohydrin Rubber | Good | Fair | Very Good | Fair | Excellent | Good |
| IIR Butyl Rubber | Good | Good | Poor | Very Good | Excellent | Fair |
| AU / EU Polyurethane Elastomer | Fair | Fair | Very Good | Poor* | Good | Excellent |
| NR Natural Rubber | Fair | Poor | Poor | Good | Poor | Excellent |
| SBR Styrene Butadiene Rubber | Fair | Poor | Poor | Good | Poor | Very Good |
What problem are you trying to solve?
Start with FFKM
Semiconductor, chemical processing, refinery and ultra-critical static seals.
Start with FKM
Fuel trains, engines, pumps, valves and hot hydrocarbon service.
Start with FEPM
Sour gas, geothermal, steam and chemical duties that punish conventional FKM.
Start with FVMQ
Aerospace and fuel systems where cold flexibility matters.
Start with HNBR
High-pressure energy service, hydraulics and mechanically demanding seals.
Start with EPDM
Water, sanitary, brake-fluid and outdoor service—away from petroleum oil.
Start with VMQ
Where flexibility, cleanliness and dry-heat performance are primary.
Start with NBR
The economical workhorse for mineral-oil and hydraulic systems.
Start with EPDM
Water, sanitary, brake-fluid and outdoor service—away from petroleum oil.
What problem are you trying to solve?
Precision O-Rings
Semiconductor, chemical processing, refinery and ultra-critical static seals.
X-Rings / Quad Profiles
Four-lobe profiles for suitable static and dynamic applications.
Gaskets & Face Seals
Custom moulded shapes, flat seals and equipment interfaces.
Rubber-to-Metal Bonded
Elastomer bonded to brass, stainless steel or engineered inserts.
Bellows & Diaphragms
Flexible components for movement, isolation and pressure response.
Hammer Union / Pressure Seals
HNBR, FKM, FEPM and other project-selected materials.
Washers, Grommets & Boots
Protection, isolation, cable, dust and equipment-interface parts.
Custom Critical Components
Micro mouldings, complex sections, inserts and precision rubber parts.
Material knowledge becomes valuable when it can be turned into a repeatable part.
Ultraswage combines elastomer know-how with tooling, precision moulding, finishing and inspection to support standard, non-standard and rapid custom requirements.
1–2000 mm ID
≤200 mm Rapid Program
60–90 Shore A
Precision Tooling
Rubber-to-Metal
Optical Inspection
Cryogenic Deflashing
Critical Industries
The failed O‑ring usually tells a story—if you know what to look for.
A replacement seal should not be chosen until the failure mechanism is understood. Specialist failure laboratories separate material failure, design failure, assembly damage and operating-condition overload because each requires a different corrective action.
Extrusion / nibbling
Pressure forces softened rubber into excessive clearance. Look for bitten or ragged material on the low-pressure side. Corrective levers include clearance, hardness, pressure, temperature and back-up rings.
Compression set / loss of force
The seal remains flattened and no longer recovers enough to maintain contact. Heat, time, cure quality and compound selection are common contributors.
Chemical swell
The O-ring increases in volume, becomes soft, sticky or distorted. The root issue is often incorrect media compatibility or a temperature-driven compatibility change.
Thermal embrittlement
Hard, cracked surfaces and loss of elongation can indicate prolonged thermal or oxidative overload.
Spiral failure
Twisting in reciprocating service creates a helical damage pattern, often related to friction, inadequate lubrication, eccentricity or groove conditions.
Abrasion
Flattened, worn or roughened surfaces indicate repeated rubbing, poor surface finish, contamination, insufficient lubrication or incorrect material choice.
Ozone cracking
Fine cracks typically form perpendicular to tensile strain in ozone-sensitive elastomers. NBR and NR require particular care in exposed storage/service.
Assembly damage
Cuts, slices or local tears can originate during installation across threads, ports, sharp edges or dry surfaces. Richter reports assembly damage as a meaningful share of real seal failures.
Rapid gas decompression
High-pressure gas diffuses into the elastomer. If pressure drops faster than gas can escape, internal blistering, splits or explosive damage can occur.
Processing / under-cure defect
Incorrect cure, contamination, knit/non-fill defects or processing cracks can compromise a seal before installation. Analytical and cross-link tests help separate material defects from service damage.
A world-class O‑ring quality system checks identity, geometry, cure state, ageing and real application behaviour.
Not every test needs to be performed on every production lot. The important point is to know which question each method answers, and to build the inspection plan around application risk.
Fast identity & finished-part control
- Dimensions: ID, cross-section and geometry against the applicable drawing/standard.
- Automated visual inspection: non-fill, flash, cuts, surface defects, foreign material and dimensional screening where applicable.
- Hardness / Micro‑IRHD: screening of finished-part hardness with geometry-aware methods.
- Density: quick incoming/identity indicator that can reveal formulation mix-ups when compared with a controlled reference.
- Surface quality: acceptance against customer criteria or ISO 3601-3 classes where specified.
Compound performance
- Tensile / elongation: strength and extensibility before and after ageing.
- Compression set: residual deformation after prescribed compression, time and temperature.
- Heat ageing: property retention after thermal exposure.
- Ozone: resistance to ozone cracking for susceptible polymer families.
- Immersion: volume, hardness, tensile and elongation changes after exposure to actual or simulated service media.
Advanced analytical verification
- FTIR: identifies polymer functional groups and helps confirm material family.
- TGA: separates major formulation fractions by controlled thermal mass loss and is powerful for compound fingerprinting.
- DSC: evaluates transitions, cold behaviour and, in some cases, residual curing reactions.
- DMA: characterises viscoelastic modulus and damping over temperature/frequency.
- Pyrolysis GC‑MS: high-resolution analytical route for identifying organic formulation ingredients when forensic depth is required.
Application qualification
- TR10 / low-temperature set: validates recovery near the cold operating limit.
- Compression stress relaxation: measures how sealing force decays with time.
- Tightness / leakage testing: verifies whether the assembled sealing system actually holds pressure after ageing or exposure.
- Rapid gas decompression: specialized qualification for high-pressure gas service.
- Customer-specific media cycling: reproduces real temperature/chemical cycles for critical applications.